1. … are used for fabrication of equipment and vessels for handling of sulfuric acid and many chloride containing media. This fluxcored wire may …
  2. … and reheat cracking. NILO Alloy 36 is available for Tig, Mig and SAW process. … NILO Alloy 36, Invar, cast Iron … NILO Alloy 36 …
  3. … CEWELD 320 was designed specifically to withstand sulfuric acid. Its nickel, chromium, molybdenum and copper levels all …
  4. … Special alloyed copper wire for Mig and Tig welding.       The weld metal is a Cu-Al bronze with high …
  5. … as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool 55ºC/ hour to 620ºC, than Air Cool for 8 hours.   … …
  6. … •       Special alloyed copper composite wire suitable for the Mig process•       The weld metal is a Cu-Al-Ni bronze with extreme …
  7. … temperature oxidation, carburization, sulfidation and to reducing-sulfurizing and metal dusting environments … ASTM B163, B166, B167, B168 …
  8. … CEWELD® 320 Tig was designed specifically to withstand sulfuric acid. Its nickel, chromium, molybdenum and copper levels all …
  9. … weld. Rapid cooling can lead to cracking, so post-weld heat treatment might be necessary. Shielding Gas : Inert gases like argon or helium … risk of cracking. After welding, slow cooling or controlled annealing might be required to minimize residual stress and prevent cracking. …
  10. … High quality alloyed copper wire for the Mig process (Mig brazing as well). The weld metal is a Copper-Aluminum bronze. …