1. … it suitable for use in oil and gas processing environments where hydrogen sulfide is present. Alloy C276 is widely used in industries …
  2. … best of each segment in the welding industry. In the past 8 years a huge number of people have visited the WSC on the seminars that are …
  3. … metal conditioned by the high-basic slag in combination with very low hydrogen content. Suitable for heat treatment. Step cooling is …
  4. … FL 851 is an agglomerated semi-basic low hydrogen SAW flux. Basicity: about 1,7 (according to Boniszewski) …
  5. … metals in more than 60 countries worldwide.  During the last decade a huge number of new alloys have been developed  by our R&D team of …
  6. … tensile ductility, and is not normally subject to strain age cracking problems common for gamma prime strengthened alloys.  … NIckel based …
  7. … stress corrosion cracking. This alloy is often chosen to solve SCC problems, which may occur with 316L stainless … 2.4660, AISI 320 UNS …
  8. … is able to Weld out of position at extreme currents and offers a Low hydrogen weld deposit. Excellent slag removal and protective gas is not …
  9. … due to its absolute insensitiveness for rust or diluted base metals. Hydrogen content: HD < 10ml/100g weld metal. … Reh ≤ 420 MPa (67 ksi) …
  10. … be used in combination with FL 851 and FL 155, both fluxes offer low hydrogen content and excellent weldabillity in multi layer welding and …