- … CEWELD® NiCu30Mn is a Nickel - Copper weld metal and has properties similar to “Monel 400”. …
- … in gases having an oxidising and sulphidising effect. Due to its high nickel content, CEWELD® SA Nicro 690 Strip is exceptionally resistant …
- … is on equal base-material scale-resistant and, by reason of its low nickel-content, resistant against attack of sulphourus gases at higher …
- … corrosion-resistance in a range of severe environments. Its high nickel (Ni) and molybdenum (Mo) provide good resistance in reducing … … Duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and …
- … up to 1149°F (2100°F), especially when welding on base metals of nickel-iron-chromium alloys. … Inconel alloys 600 and 601, Incoloy …
- … low level of free carbon and enables the filler metal to be used with Nickel 201. The weld metal has good corrosion resistance, particularly … in alkali’s. … CEWELD® NiTi 3 is developed for welding and cladding Nickel 200 and Nickel 201. This alloy is also suited for surfacing of steel. …
- … This Nickel - Copper weld metal has properties similar to “Monel 400”. It …
- … weld deposit composition of 59%Ni-23%Cr-16%Mo is designed to match the nickel base corrosion resistant alloy commonly known as alloy 59. The … and Superduplex stainless steels or combinations of these with nickel base alloys. Some authorities do not allow or have discontinued … … duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C4, C-276, …
- … against fouling. Suitable for dissimilar welding of Monel Alloy 450 to Nickel 200 and or other Copper -Nickel alloys. Small diameters can be used in all positions. … Cu7158 … (Monel 67): Wrought and Cast Alloys of 70-30, 80-20 and 90-10 Copper Nickel Alloys, Monel Alloy 450, Nickel 200, CuNi10Fe, CuNi20Fe …
- … 320 Tig was designed specifically to withstand sulfuric acid. Its nickel, chromium, molybdenum and copper levels all provide excellent … environments, normally without post-weld heat treatment. At 33% nickel, CEWELD® 320 Tig has practical immunity to chloride stress …