1. … covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and …
  2. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., 99,5, 3.0205, …
  3. … low heat input and the interpass temperature should be limited to max. 150 °C. … 1.4898, GX45NiCrNbSiTi45-35  Parralloy H46M, Centralloy ET45, …
  4. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, Al99,0 …
  5. … on operating system compare to overlay welded plates. Manageable size (150x100x5mm), easy to transport and easy to apply in all positions More …
  6. … anodizing. Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … AlMgSi 0, AlSiMg (A), AlSi 1 MgMn, …
  7. … with good corrosion and acid resistance. Scale resistance up to 1150ºC, crack and wear resistant, suitable for rebuilding wornout parts. …
  8. … Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11, G-AlSi12 (Cu), …
  9. … Recommended for operating temperatures up to 1150° C in carburized low-sulphur combustion gas, e. g. reforming ovens …
  10. … be kept below 15 kJ/cm and interpass temperature between 100 and 150ºC. … S690, X80, X90, X100, S690QL1, Weldox 700, Dilimax, Naxtra 70, …