1. … resistant up to 950ºC. Interpass temperature should be kept below 150ºC.  … 1.4828, 1.4829, 1.4893, 1.4835, 1.4818, 1.4825, 1.4826, …
  2. … Recommended for operating temperatures up to 1150° C in carburized low-Sulphur combustion gas, e. g. reforming ovens …
  3. … for working temperatures between -196 °C and +650 °C. Recovery 150% with excellent arc stability and easy slag removal. … Dissimilar …
  4. … metal provides optimum strength and oxidation resistance above 816°C (1500°) up to 1149°F (2100°F), especially when welding on base metals of …
  5. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good corrosion-resistance and …
  6. … seawater. Welding instructions: - Preheating for sections >6 mm from 150 till 300 ºC is recommended. Use the normal standard welding …
  7. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., 99,5, 3.0205, …
  8. … covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and …
  9. … low heat input and the interpass temperature should be limited to max. 150 °C. … 1.4898, GX45NiCrNbSiTi45-35  Parralloy H46M, Centralloy ET45, …
  10. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, Al99,0 …