1. … be kept below 15 kJ/cm and interpass temperature between 100 and 150ºC. … S690, X80, X90, X100, S690QL1, Weldox 700, Dilimax, Naxtra 70, …
  2. … in concentrated (98.5 %) sulphuric acid at temperatures of up to 150 °C (300 °F). … CEWELD® SA Nicro 690 Strip is mainly used for ESW …
  3. … exceeded. The working temperature should be between 100°C (212 °F) and 150°C (302 °F) . As welding flux FL 155 should be used because of its …
  4. … up to much higher temperatures. Preheating is recommended at 150 - 350° C. depending on the thickness of the base metal. Similar …
  5. … against attack of sulphourus gases at higher temperatures up to 1150 °C. When welding CEWELD 4820 AC low heat-input is required as …
  6. … aluminium grades. Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the benefits of …
  7. … metal provides optimum strength and oxidation resistance above 815 °C (1500°F) up to 1149 °C (2100°F), especially when welding on base metals …
  8. … Weld metal provides optimum strength and oxidation resistance above 1150 °C ( 2100 °F), especially when welding on base metals of …
  9. … things that effects the quality, some wires have strength of more than 1500 MPa and some wires only have 600 MPa but why is this so important? …
  10. … prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good corrosion-resistance and …