- … Low spatter loss, easy slag removal. Suitable for economic welding of Mo-steels up to 500°C (932°F). … Typ 0,5Mo ≤ 460 MPa, ISO …
- … deposits are air-hardenable that can normally be heat-treated after welding … 1.4000, 1.4001, 1.4002, 1.4003, 1.4006, 1.4008, 1.4021, …
- … a slightly higher percentage of phosphor, suitable for MIG welding, easy to handle, high plasticity of the weld metal. High …
- … Designed for welding heat resistant steels to sustain working temperatures up to …
- … yield strength up to 420 MPa. It is particularly suitable for welding on AC and DC+. CEWELD® E 7018-1 is suitable for steels with up …
- … CEWELD® FL 400 is an agglomerated flux for SAW welding to obtain increased hardness with low and un-alloyed sub arc …
- … hot cracking resistance and mechanical properties. To be used with welding flux FL 8111 or FL 838 … 1.4507, 1.4410, 1.4468, 1.4515, …
- … Suitable for downhand butt- and fillet weld, smooth welding pool without spatter loss, easy slag release, very nice bead …
- … Flux has a low hydrogen potential which makes it suitable for overlay welding of heat resistant steel like A387 types. … Cr, CrNi, CrNiMo …
- … SG CrMoV6 (EN 4334: FE-WL1806 (15CrMnMoV5-4-9-3) wire is used for welding matching, and similar, composition base materials. The …