1. … A continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. …
  2. … in chloride-bearing solutions (a form of degradation to which the austenitic stainless steels are prone). It is able to withstand a wide …
  3. … and scale resistance than the standard L-type. The microstructure is austenite with approx. 5-10% ferrite. … ISO 15608: 8.1  Austenitic ≤ 19 % Cr 9 % Ni, TÜV 1000: Gr. 21,  1.4301,  1.4308, …
  4. … All our seamless fluxcored welding wires undergo a full 3.1 all weld metal test according EN 1597. In addition …
  5. … DC. The carbon content of the base metal should not exceed 0,45 % in order to avoid lack of fusion.  … Scratchers, Mixers, Deep drilling, …
  6. … offers a easily machinable weld deposit with high ductility and no undercut. … Welding ductile, grey and malleable cast irons. Ni 99 can …
  7. … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …
  8. … industries. It is used for combustion cans, transition ducts, flame holders, thermocouple sheaths, and other important gas turbine components. …
  9. … fluidity (wetting action), making the alloy the preferred choice of welders. The alloy is not sensitive to weld cracking and produces bright, …
  10. … improved high temperature creep properties. The weld deposit is fully austenitic and corrosion resistant. … ISO 15608: 8.1  Austenitic ≤ 19 % Cr , TÜV 1000: Gr. 21-30 1.4335 , 1.4435  1.4465 , …