1. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …
  2. … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by …
  3. … μm FSSS Apparent density (ISO 3923-2) 5.2-5.8 g/cm³ Particle shape: preponderantly spherical Coating microhardness: 800-1300 HV0.3 Sales … 3.3): -45+22 μm (*other sizes on request) -38+15 μm -25+10 μm … Compressor shafts, pump seals, flap actuators, paper rolls, ball valves, …
  4. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low …
  5. … High pressure resistance and high wear resistance. The alloy is …
  6. … in a strong and innovative brand? Then please   contact us for preliminary talk. … Becoming a Dealer …
  7. … ER409 alloy. Single pass welds on light gage base metal or welds with preheat do not usually require PWHT. … 1.4000, 1.4002, 1.4016, 1.4057, …
  8. … Alloy 740H is a nickel-base, precipitation hardenable superalloy that offers a unique combination of …
  9. … your questions. Improving the website and adapting the content to your preferences. Resolving technical problems and ensuring security. …
  10. … 10 KJ/cm. Cooling time (T8/5) must be adjusted by travel speed and preheat temperature. … S890 TM-pipe steels to StE 890 to S890QL1, A …