1. … temperatures up to 600°C. The weld metal is resistant to high hydrogen pressure. … 12crmo19.5, GS-12crmo19.5, 1.7362, 1.7363     … E CrMo5 … A …
  2. … and well suited for low-temperatures, ductility down to -60°C. Preheating, interpass temperature and post weld treatment as required … 1.8914, 1.8927, 1.8931, 1.8928, 1.7147, 1.7149, 1.8734 S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1, 20MnCr65, 28CrMn4-3 L480 - L550, X65, X80, …
  3. … as permanent stress by heat influence, metal wear and high surface pressure  … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …
  4. … current, copper coated core wire and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  5. … that leaves a clean surfaceSound deposits are obtained even in the presence of cross draughtsPrimary choice for cladding and rebuilding …
  6. … in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing …
  7. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. Outstanding slag release. … Rebuilding worn …
  8. … of up to 550°C. Typical applications are in power plant construction, pressure pipe, turbine and boiler construction. The alloy is also used …
  9. … Seamless flux-cored wires represent a remarkable innovation in the field of welding, particularly …
  10. … The presence of tin improves the fluidity is useful to increase the …