1. … that leaves a clean surfaceSound deposits are obtained even in the presence of cross draughtsPrimary choice for cladding and rebuilding …
  2. … and well suited for low-temperatures, ductility down to -50°C. Preheating, interpass temperature and post weld treatment as required …
  3. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. Outstanding slag release. … Rebuilding worn …
  4. … elevated temperatures. Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11, G-AlSi12 …
  5. … hydrogen in 100gr weld metal is exceeded. The most important steps to prevent hydrogen induced cracking are: 1)  Use airtight packing for …
  6. … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by …
  7. … Seamless flux-cored wires represent a remarkable innovation in the field of welding, particularly …
  8. … The presence of tin improves the fluidity is useful to increase the …
  9. … grain growth in Weld Metal zones (WM) due to titanium nitride (TiN) precipitation in the still liquid metal in these zones, thus avoiding …
  10. … down hand welding. Excellent against pitting and stress corrosion. The PREN above 35 weldmetal offers outstanding resistance against pitting. …