1. … exhibits outstanding resistance to pitting and crevice attack in the presence of chlorides and other halides. … Alloy C-2000 … Alloy C-2000 …
  2. … High pressure resistance and high wear resistance. The alloy is …
  3. … metal requires no buffer layer. Suited for wear parts subject to heavy pressure, impact and shock. The interpass temperature should be maximum …
  4. … 4.2-5.5 g/cm³ (dependent on designated size) Particle shape: preponderantly spherical Typical grain size for sale: -53+22 μm ask for …
  5. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good …
  6. … your questions. Improving the website and adapting the content to your preferences. Resolving technical problems and ensuring security. …
  7. … used on the back surface of sheet or plate less than 1/4 in. thick to prevent oxidation. Gas Requirements. Welding-grade argon (99.999 …
  8. … Welding procedure (including preheat temperature, interpass temperature and PWHT) will be dependent … kept below 15 kJ/cm and interpass temperature between 100 and 150ºC. … S690, X80, X90, X100, S690QL1, Weldox 700, Dilimax, Naxtra 70, 10CrMo9-10, 16NiCrMo12-6, high …
  9. … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300 - 400 °C. Old Hardfacing layers should …
  10. … Can be welded crack free by preheating approxiamately 450°C and keep that also as interpass … for example in an oven. … 56-59 HRc hardfacing alloy, Mixing peddles, Press screws, Kneading machine, screw conveyors, pumps etc. … OA 54 L … …