1. … alloys and covers a weight range of alloys. Thicker sections should be preheated (150°C) prior to welding. Qualified by Lloyds for manual and …
  2. … extreme high strength with excellent ductility and good weldabillity. Preheat and interpass temperature > 200°C …  1.7218, 1.7225 25 CD4, 13 …
  3. … of the pure aluminium grades. Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the …
  4. … hardness and is resistant against metal-metal wear and high surface pressure.  … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …
  5. … as most commercial copper grades. Thicker sections than 5 mm should be preheated up to approximately 500 °C. … Cladding steel, Grey cast iron, …
  6. … suited for welding jobs at poorly accessible points and badly prepared seams. CEWELD® E 6013 S can be sued in all positions, in …
  7. … type for economic production of creep resistant steels and pressure-hydrogen-resistant 2¼Cr1Mo-steels. Due to the seamless …
  8. … cobalt-based alloys, allowing multiple layer build-ups with no pre-heating needed. -ULTIMET wire produces deposits wich harden quickly …
  9. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150 °C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., …
  10. … setup and our ProHeat 35 induction machine with Rolling Inductor, for preheating the manipulator. In addition to performing these processes …