1. … Use the form down below to request your password. … Request password …
  2. … layer welding in general construction with good cold tough properties down to -40 degrees Celsius. Basicity according to Boniszewski:Grain …
  3. … out-of-position welding also at higher currents. Using temperature down to - 40 °C. Particularly suited for MAG-orbital welding and …
  4. … level between 30 and 50 (FN). Excellent for use in position and down hand welding. Excellent against pitting and stress corrosion. The …
  5. … Lower preheat and interpass temperatures are possible, yet must be approved by practical welding tests and process qualification tests. …
  6. … and excellent slag removal.Excellent for use in horizontal and down hand position … ISO 15608: 8.1  Austenit ≤ 19 % Cr 9 % Ni, , TÜV …
  7. … All CEWELD® products are listed in this brochure downloadable as PDF. … Catalogue …
  8. … a high polish. CEWELD E 4430-Ti Fall is designed to weld in vertical down position (PG) and offers a fast freezing slag that makes it also …
  9. … used in high demanding applications, we are proud to be the pioneer in offshore and heavy construction and we thank our customers for choosing …
  10. … positions for diameters 2.4 and 3.2mm. Diameters < 4.0mm excellent in down position. … Joining Duplex, Superduplex, super austenitic …