1. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast … EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350, GG10, GG15; GG20, GG25; GG30; GG35; GG40 EN 1562: EN-GJMB-350, EN-GJMB-550 , EN- GJMW-350, EN- GJMW-550 , GTS 35, GTS 55, GTW 35, …
  2. … of the year 2015 in the district called "The Betuwe". It all happened during a exiting campaign evening of "Betuwe onderneemt Beter", Monday …
  3. … in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing peddles, …
  4. … alloy containing Nickel for more strength and bridging capability during brazing with excellent rebuilding properties.  Flux/Paste: …
  5. … that this steel is distinctly vulnerable to sensitization phenomenon during welding, even though martensite hogs a great amount of carbon …
  6. … Good resistance against hot cracking due to the high Mo content. During build-up welding, the weld metal already achieves approximately …
  7. … and leaves a fine rippled shiny surface. Max. service temperature 350ºC. Corrosion resistance similar to low carbon CrNiMo(Mn,N)-steels. …
  8. … For the best results, welding must be done in a low heat input procedure and is not recommended for multi-pass applications … 1.4512,  …
  9. … resistance to intercrystalline corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon …
  10. … less than 1% nickel to full fill NACE requirements and cover more procedures up to 500 MPa yield strength steels. CEWELD® AA M500 can also be … L360NB, L415NB, L360MB-L450MB, L360QB-L450QB ASTM A 203 Gr. D, E; A 350 Gr. LF1, LF2, LF3; A 420 Gr. WPL3, WPL6; A 516 Gr. 60, 65, 70; A … 65, Oceanfit 355, Oceanfit 420, Oceanfit 460, alform plate 460M; durostat 400, 450, 500, durostat B2     … AA M500 … A 5.28: E80C-Ni1 H4 …