1. … parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the benefits of being relatively …
  2. … crack resistant alloy with high mechanical properties and excellent welding characteristics. High impact strength at sub zero temperatures …
  3. … Cr and Mo-alloyed basic elektrode for welding creep resistant steels and steel casting for working temperatures …
  4. … against hot cracking due to the high Mo content. During build-up welding, the weld metal already achieves approximately the composition of …
  5. … metal has low levels of tramp elements (eg. Sn, As, Sb and P) providing a low Bruscato Factor(X < 10 ppm)for temper embrittlement …
  6. … particle distribution. The spray deposit is only machinable by grinding with diamond tools. … Cement industry, pumps, mixer blades, valves …
  7. … The Ceweld AA 904L is used for welding materials of similar chemical composition which are used for …
  8. … above 816°C (1500°) up to 1149°F (2100°F), especially when welding on base metals of nickel-iron-chromium alloys. … Inconel alloys …
  9. … resistance against seawater and general corrosion with excellent welding properties with self detaching slag.  … NF A 35-578 : Z 15 CN 24.13 ASTM/AISI : 304, 347, 309 DIN 17175 : X 12 CrNi 22.12. W.Nr: 1.4828, 1.4311, 1.4712, 1.4742. …
  10. … hot cracking resistance and mechanical properties. To be used with welding flux FL 8111 or FL 838 … 1.4507, 1.4410, 1.4468, 1.4515, 1.4517, …