1. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. Outstanding slag release. … Rebuilding worn …
  2. … to be used in corrosive environments, normally without post-weld heat treatment. At 33% nickel, CEWELD 320 LR has practical immunity to …
  3. … reduces the tendency to crack, especially if the weld seams are not heat-treated.These steels are usually used for operating temperatures … to temper embrittlement. … For similar 1.25%Cr-0.5%Mo-alloyed, heat-resistant, ferritic steels. 1.7335, 1.7242, 1.7337, 1.7357 13CrMo …
  4. … AA M610 can also be used for constructions that needs post weld heat treatment after welding and still offers excellent impact …
  5. … CEWELD AA M500 can also be used for constructions that needs post weld heat treatment after welding and still offers mechanical properties …
  6. … dissimilar welding between cast iron and high alloyed stainless and heat resistant steels or mild steels. Excellent Weldabillity with …
  7. … reduces the tendency to crack, especially if the weld seams are not heat-treated.These steels are usually used for operating temperatures … to temper embrittlement. … For similar 1.25%Cr-0.5%Mo-alloyed, heat-resistant, ferritic steels. 1.7335, 1.7242, 1.7337, 1.7357 13CrMo …
  8. … non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  9. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Slag crushers, Sugar cane knives, Hammers, …
  10. … Mechanical properties listed below reflect utilization of a post-weld heat treatment between 1020°C (1875°F) and 1050°C (1925°F) for one …