1. … be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or …
  2. … to heavy impact and shock. The interpass temperature should be maximum 250ºC. The weld metal is machinable by special carbide tools, hardening …
  3. Type C Mn Si Cr Ni Mo Nb N W Other PREn 307 Si <0.12 6.5 0.8 18.5 8.5           19 308 LSi <0.03 1.7 0.8 21.0 10.0 <0.75         19 308 H <0.03 1.7 0.8                 309 LSi 0.05 1.8 0.45 21.0 10.0 <0.5           309 H <0.12 1.8 0.5 24.0 13.0             310 0.10 1.8 0.5 26.0 21.0 <0.3           …
  4. Brand: Selectarc
    CEWELD Product: 2594 Super Duplex
    52 … SELECTARC D25/09W …
  5. Brand: Selectarc
    CEWELD Product: AA 2594
    … 52 … SELECTARC FCW 2509MO …
  6. Brand: Avesta
    CEWELD Product: SACW 2594 Super Duplex
    … 36 … 2507/P100 …
  7. CEWELD Product: E DUR 300 Kb
    … 275 … HARDMELT 250
  8. CEWELD Product: SG CrMo1
    … 45 … Lastek 250C …
  9. Brand: Lincoln Electric
    CEWELD Product: E NiCrMo 686 CPT
    … 46 … Jungo SD 2509 …
  10. Brand: Selectarc
    CEWELD Product: 4501 Kb
    … 52 … Selectarc INOX 2509MoWB …