1. … to avoid cracking. A buffer layer with AA M690 or AA M37-42 is recommended in case of sensible base material or old hardfacing layers. … HRc …
  2. … More than 1 layer should not be deposited. A Buffer layer is recommended in case of sensitive base material or old unknown layers. OA 67 …
  3. … of any welding consumable and procedure before use in the intended application.  The selection and use of specific products is …
  4. … coating structure, all spray metal requires no buffer layer. Recommended for coatings against erosion and corrosion and ingreased …
  5. … very high resistance to cracking due to its high elongation. We recommend CEWELD FL 880 or FL 838 as welding flux … 19%Cr,  9%Ni Type, ISO …
  6. … carbide tip tools, hardening is possible. The maximum hardness is dependent on the base metal and is usually already achieved in the first …
  7. … oxidation and abrasion, and excellent resistance to impact and bending. SP 80/20 NiAl can be machined and ground to a finish of 5 micro …
  8. … coatings on steel substrates. Furthermore, the aluminum coating tends to form an oxide film that protects it from further attack. … … on components such as conductive areas on insulators, capacitor end caps and varistors. Cathodic corrosion protection on steel, …
  9. … not be deposited. A Buffer layer with OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. Equivalent in …
  10. … The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall a temperature of 1000°C be …