1. … to avoid cracking. A buffer layer with OA 4370 or OA MnCr is recommended in case of sensible basematerial or old layers. Weldable without …
  2. … where high temperature properties are required. It is not recommended to use this alloy for welding aluminium alloys with a high …
  3. … layer. A buffer layer with CEWELD® OA 4370 or CEWELD® OA MnCr is recommended in case of sensible basematerial or old hardface-layers. Weldable …
  4. … or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing layers should be removed, clean or …
  5. … minimize the heat input, because materials of this composition have a tendency to embrittle in the temperature range of approx. 600-800° C. …
  6. … low alloyed steels with tensile strength up to 510 N/mm2. Recommended for root welding in pipelines due to excellent welding …
  7. … resistance against organic and non-oxidizing acids and are recommend for internal and external diameters. Using the combustion wire …
  8. … Filler metal specifically intended for high integrity structural service at elevated temperature so …
  9. … thanks to the Titanium carbides. The choice for the buffer layer is depending on the base metal and not always necessary.  … HRc 54-59, …
  10. … long term creep properties. These consumables are specifically intended for high integrity structural service at elevated temperature so …