1. … Preheating and interpass temperature 400-450 °C (austenitic welding) or 250-300 °C (martensitic welding). Root passes should …
  2. … NiCrMo 686 (UNS N06686/W.Nr. 2.4606) is a single-phase, austenitic Ni-Cr-Mo-W alloy offering outstanding corrosion-resistance in a … than competitive materials. … Duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, …
  3. … Fully austenitic weld metal with high resistance against stress corrosion cracking …
  4. … Excelent weldabillity with fully austenitic weld metal with high resistance against stress corrosion cracking …
  5. … A high basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo …
  6. … Austenitic deposit with strain hardening properties and no limmits in the …
  7. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat … down to -196°C. Good resistance to nitric acid. … ISO 15608: 8.1  Austenitic ≤ 19 % Cr 9%Ni , TÜV 1000: Gr. 21 - 22 (29 max.350°C), … 6 CrNi 18 9, X 12 CrNi 18 9, G-X 8 CrNi 18 10, X 6 CrNi 18 10, X 10 CrNiTi 18 10,  X 5 CrNi 18 10 AISI 304, 304H, 312, 321H, 347, 347H,  UNS …
  8. … High wear resistance and austenitic structure deposits. The deposit gives already a very good …
  9. … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. CEWELD 4842 Kb has good … high temperatures, due to its high Cr content. The alloy is fully austenitic and is therefore sensitive to hot cracking. The temperature …
  10. … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. AA 310B has good general … high temperatures, due to its high Cr content. The alloy is fully austenitic and is therefore sensitive to hot cracking. The temperature … thermic shock, and is superior to type 309L … ISO 15608: 8.1  Austenitic ≤ 19 % Cr , TÜV 1000: Gr. 21-30,  Type: 25% Cr, 22%Ni  1.4710, …