1. Brand: Selectarc
    CEWELD Product: ER 90S-B3
    … Existe en TIG  … 52 … SELECTARC F68 …
  2. … steels that have to fullfill impact requirements down to -60 degrees Celsius and parts that have to be soft annealed above 900 degrees Celsius. Suitable for use with FL 155 agglomerated flux or with FL CS155 …
  3. Brand: Castolin Eutectic
    CEWELD Product: AA SS 50
    … or CastoWIG 45301 W / CastoTig 45301 W TiG … 38 … Casto 45301 …
  4. … stainless steels and Nickel based alloys: AISI 308L, 347, 316L, 309L and 309LN. Basicity: About 1,9 (according to Boniszewski) Current: DC or …
  5. … Usually combined with AlSi12 or AlSi5 filler metal. … Brazing for Aluminium and Aluminium Alloys with a working range from 350 to 550 °C. Usually combined with AlSi12 or AlSi5 filler metal. … Alu-Flux … 18496: FL20 …
  6. … are different welding methods you can use for magnesium, including TIG (Tungsten Inert Gas) welding and laser welding. TIG welding is a common choice, as it allows for precise control of … Gas : Inert gases like argon or helium are used as shielding gases in TIG welding to prevent oxidation during the welding process. A …
  7. … VDM Alloy 690, Nicrofer 6030 N, FM 52, 2.4642, NiCr29Fe … NiCro 52M Tig … A 5.14: ERNiCrFe-7A … 18274: S Ni 6054(NiCr29Fe9) …
  8. Brand: Selectarc
    CEWELD Product: 410 NiMo Tig
    … 52 … SELECTARC M13/4 TIG
  9. … - OF-Cu, 2.0070 - SE-Cu, 2.0076 - SW-Cu, 2.0090 - SF-Cu … CuAg (LP) Tig … A 5.7: ERCu … 24373: Cu 1897 / CuAg1 …
  10. … : GGG-40, 50, 60, 70. DIN 1692 : GTS-35, 45, 55, 65, 70. … NiFe 55 Tig … A 5.15: E NiFe-CI … 1071: SC NiFe-1 …