1. … offers a easily machinable weld deposit with high ductility and no undercut. … Welding ductile, grey and malleable cast irons. CEWELD® …
  2. … layer in case off multi-layer welding. The weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in …
  3. … alter the surface electrochemistry of the material in the crevice or under a surface deposit. Grade 12 has better elevated temperature …
  4. Austenitic filler metal for stabilized and non-stabilized CrNi steels. … down to -196°C. Good resistance to nitric acid. … ISO 15608: 8.1  Austenitic ≤ 19 % Cr 9%Ni ,TÜV 1000: Gr. 21 - 22 (29 max.350°C), …
  5. … kwaliteitscontrolemaatregelen. Ons uitgebreide aanbod aan ultramoderne testapparatuur is een bewijs van ons streven naar uitmuntendheid. …
  6. … all spray metal requires no buffer layer except on materials considered critical. In this Situation Ceweld SP NiAl is recommended. Suited …
  7. … in chloride-bearing solutions (a form of degradation to which the austenitic stainless steels are prone).It is able to withstand a wide …
  8. … all weld metal requires no buffer layer except on materials considered critical or in case of old hardsurfacing layers. The weld deposit …
  9. … flowing properties and capillarity.  Colour very similar to brass. Soldering seam can be easily electroplated. Self pickling on copper to …
  10. … CEWELD E NiFe 2 has a few benefits compare to other “FeNi” types because of improvements, such as: weldable with very low current, non …