1. … staan garant voor zeer stabiele mechanische waarden zelfs na langdurig gloeien. Deze elektrode is bovendien door DNV gekeurd in de …
  2. … from porosity due to the special shaving process and cleaning method during production. AlMg4,5Mn is one of the highest grades within the …
  3. … "NiLo'" and offer the lowest schrinkage possible to avoid cracks during heating and the cooling period. The weld deposit also retains … EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350, GG10, GG15; GG20, GG25; GG30; GG35; GG40 EN 1562: EN-GJMB-350, EN-GJMB-550 , EN- GJMW-350, EN- GJMW-550 , GTS 35, GTS 55, GTW 35, …
  4. … en voor de ontwikkeling van nieuwe, innovatieve lasprocessen en -procedures. De locatie (600 m2) biedt ruimte voor de meest hoogwaardige en …
  5. … range that enables you to use only one wire to cover more procedures up to 550 MPa yield strength steels. It can also be used for …
  6. … Tempered 560° C ~ 52 HRc Tempered 450° C ~ 49 HRc Tempered 350° C ~ 48 HRc Soft annealed 250 HB … 45-52 HRc  1.2567, 1.2365, …
  7. … for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to … 15608: 8.1  Austenit ≤ 19 % Cr 9%Ni , TÜV 1000: Gr. 21 - 22 (29 max.350°C), 1.4301, 1,4306, 1.4307, 1.4308, 1.4311, 1.4312, 1.6900, 1.6901, …
  8. … from porosity due to the special shaving process and cleaning method during production.  Thicker sections should be preheated (150°C) prior …
  9. … resistance to intercrystallin corrosion and wet corrosion up to 350°C (662 °F). Corrosion-resistance is similar to low-carbon CrNiMo …
  10. … Weldable without protective gas.Corresponding electrode: CEWELD® Dur 62 S … 61-64 HRc hardfacing alloy, Cement, Mineral mixing, hammers, …