- … slag in combination with very low hydrogen content. Suitable for heat treatment. Step cooling is possible. High reserve of toughness and …
- … copper coated core wire and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
- … and DC+ with a recovery of 200% for excellent deposit performance. (Preheating is not required)Equivalent in FCAW: OA 59, OA 60 Mo, OA 61, OA …
- … was originally targeted for use as A-USC boiler tubes in the superheater sections of these plants but was then adapted for application as …
- … to be used in corrosive environments, normally without post-weld heat treatment. At 33% nickel, CEWELD® 320 Tig has practical immunity …
- Brand: ITW Elga - Hobart… content (≈2 ml/100gr) even after many years of storage. Due to less preheating required huge savings can be made and these type of wires offer …
- … wires. Excellent weld metal quality and X-ray soundness. Post weld heat treatment (PWHT) can be applied without any problems. … 19% Cr / …
- … For welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. AA …
- … with lower silver containing Phosphor-Copper Alloys. Ideal where the heat feeding is critical because of its low operating temperature. …
- … hardness of 49-53 HRc at room temperature. The weld deposit is high heat resistant up to 900°C. DUR 12 offers a low coefficient of friction …