1. … CEWELD 308H Tig has been developed for typical operating temperatures up to 400ºC, … range. It also shows good resistance to general corrosion. CEWELD 308H Tig shows higher temperature and scale resistance than the standard … UNS S30409, S32109, S34709, S30400, S32100, S34700 … 1.4302 … 308H Tig … A 5.9: ER308H … 14343-A: W 19 9 H …
  2. … • High quality alloyed copper wire for the Tig process (Mig brazing as well) • The weld metal is a Copper- Silicon … - CuZn 15, 2.1322 - CuMg 0,4, 2.1323 - CuMg 0,7 … 2.1461 … CuSi3 Tig … A 5.7: ERCuSi-A … 24373: Cu 6560 / CuSi3Mn1 …
  3. … High quality alloyed copper wire for the Tig process (Tig brazing as well). The weld metal is a Copper-Aluminum bronze.  … AISI 304, sliding Surface, shafts, bearings etc. … 2.0921 … CuAl8 Tig … A 5.7: ERCuAl-A1 … 24373: Cu 6100 / CuAl7 …
  4. … CEWELD® ER 80S-B3L Tig is a low alloy copper-coated TIG rod with 2.25% Cr and 1% Mo content, with low carbon content (less … 10H2M, B.S. grade 45, K21390, K21590, J22091, J21890 … ER 80S-B3L Tig … A 5.28: ER80S-B3L … 21952-B: W 2C1ML …
  5. … CEWELD® AlSi12 Tig was originally developed as a brazing alloy to take … 3.2163, 3.2371, 3.2151, B 413.0, 361.0, 359.0, 356.0, 319.0, Cast aluminium … 3.2885 … AlSi 12 Tig … A 5.10: ER4047A … 18273: S Al 4047A (AlSi12(A)) …