1. … to 950°C. Preheating at 250 °C and stress relieving at 800 °C is recommended if this is permissible for the base metal. In the machined state …
  2. … A Buffer layer with CEWELD® OA 4370 or CEWELD® OA MnCr is recommended in case of old layers or critical base metals. Weldable with M21 …
  3. … Recommended for operating temperatures up to 1150° C in carburized …
  4. … already a High hardness in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without …
  5. … Solution Center of B2B evenementen neem contact op met: Patrick Bovendeerd Tel: +31 (06) 54 68 2770 E-mail: info@certilas.nl   … Contact …
  6. … hardness in the first layer. The choice for the buffer layer is depending on the base metal and not always necessary.  … 55-57 HRc …
  7. … The alloy has a low carbon content which makes it particularly recommended when there is a risk of intergranular corrosion. can  be used …
  8. … ultramoderne testapparatuur is een bewijs van ons streven naar uitmuntendheid. Zo garandeert onze apparatuur de superieure kwaliteit van onze …
  9. … Equivalent) is over 40. Ar-CO2 mixed gas or 100%CO2 is recommended as shielding gas for excellent weldability. … 1.4507, 1.4410, …
  10. … - Preheating for sections >6 mm from 150 till 300 ºC is recommended. Use the normal standard welding techniques. … Aluminium bronze, …