  • PRODUCT SPECIFICATIONS
  • PACKAGING
Type
High recovery, Corrosion-resistant stick electrode without nickel. (Type 430, 1.4015)
classification
AWS
A 5.4: E 430-26
EN ISO
3581-A: E 17 B 42
W.Nr.
1.4015
Applications

CEWELD 4015 HL-Kb is used for joining and cladding 17% chromium alloys and cladding components where heat and corrosion resistance is required. Areas of application are sealing surfaces on gas, water and steam fittings.

Type
High recovery, Corrosion-resistant stick electrode without nickel. (Type 430, 1.4015)
Applications

CEWELD 4015 HL-Kb is used for joining and cladding 17% chromium alloys and cladding components where heat and corrosion resistance is required. Areas of application are sealing surfaces on gas, water and steam fittings.

Properties

CEWELD 4015 HL-Kb can withstand working temperatures of up to 450°C and offers scaling resistance up to 950°C. Preheating at 250 °C and stress relieving at 800 °C is recommended if this is permissible for the base metal. In the machined state there should be at least two weld layers on top of each other. The weld metal can be polished and is scale-resistant up to 900°C.

The achievable hardness of the weld metal is mainly influenced by the dilution with the respective base material and its chemical composition. The higher the dilution and the C content of the base material, the higher the hardness of the weld metal.
The preheat and interpass temperature should be 200 – 300ºC.
A tempering 730 – 800ºC is possible.

Classification
AWS
A 5.4: E 430-26
EN ISO
3581-A: E 17 B 42
F-nr
1
FM
5
W.Nr.
1.4015
Suitable for

1.4000, 1.4002, 1.4016, 1.4057, 1.4740, 1.4742, 1.4057, 1.4059, 1.4741, 1.4509, 1.4510, 1.4511, 1.4512, 1.4520, 1.4712, 1.4713, 1.4724, 

X7Cr14, X12Cr13, X17CrNi16-2, X6Cr13, X6CrAl13, X6Cr17, X17CrNi16-2, X2CrTiNb18, X3CrTi17, X3CrNb17, X2CrTi12, X2CrTi17, X10CrSi6, X10CrAlSi7, X10CrAlSi13, X10CrAlSi18

UNS S40300, S40500, S40900, S41000, S42900, S43000, S43035, S43036, S43100, S44200 

AISI 403, 405, 409, 410, 429, 430, 430Cb, 430Ti, 439, 431, 442

Approvals
CE
Welding positions
PA
PB
PC
PF
Redrying
300°C / 2 hr
Analysis
C Si Mn P S Cr Ni Mo Nb N Cu Ta Nb+Ta W
0.09 0.7 0.9 17 0.4 0.3
Mechanical Properties
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Hardness
760°C±15°C 1h 360 540 22 200 HB
As Welded >300 >450 >20 250 HB
17 percent chromium stick welding electrode
17 percent chromium stick welding electrode
Packing info
4015 HL-Kb 3,2 x 350mm
Packaging KG/unit EanCode
Can 2,6 8720663415554
4015 HL-Kb 4,0 x 350mm
Packaging KG/unit EanCode
Can 2,6 8720663415561