CEWELD 25-35Nb Tig

Product category
Type
Filler metal for heat resistant stainless steel with simmilar composition
Applications
Joining and cladding high heat resistant CrNi-steels of the same kind and Cast steels in a low sulphourus invironment.
Properties

Recommended for operating temperatures up to 1150° C in carburized low-Sulphur combustion gas, e. g. reforming ovens in petrochemical plants.

Classification
EN ISO
14343-A: W Z 25 35Nb
DIN: W.Nr.
~1.4853
F-nr
6
FM-nr
5
Suitable for

1.4852, 1.4853,  1.4857, 1.4837, 1.4849, 1.4848

G-X40NiCrNb35-25, G-X40CrNiSi25-12, G-X40CrNiSi25-20, G-X40 NiCrSi35-25,  G-X40NiCr38-18, G-X40NiCrNb35-25, cast steels, HK40, HK45, Incoloy 800H

UNS: J93503, J94204, N08705

Manaurite 36X

Approvals
CE
Welding positions
Redrying temperature
Not required
Gas acc. EN ISO 14175
I1
Analysis
C Si Mn P S Cr Ni Mo Nb N W Cu Ti
0.4 0.8 17 0.01 0.01 26 35 1.4 0.1
Mechanical Properties (typical)
Heat
Treatment
RP0,2
(N/mm2)
Rm
(N/mm2)
A5
(%)
Hardness
As Welded 480 700 8 0 HRc