1. … 4.2-5.5 g/cm³ (dependent on designated size) Particle shape: preponderantly spherical Typical grain size for sale: -53+22 μm ask for …
  2. … exhibits outstanding resistance to pitting and crevice attack in the presence of chlorides and other halides. … Alloy C-2000, 2.4675, …
  3. … and cleaning method during production.  Thicker sections should be preheated (150°C) prior to welding. … Filler metal for welding …
  4. … Welding procedure (including preheat temperature, interpass temperature and PWHT) will be dependent … kept below 15 kJ/cm and interpass temperature between 100 and 150ºC. … S690, X80, X90, X100, S690QL1, Weldox 700, Dilimax, Naxtra 70, 10CrMo9-10, 16NiCrMo12-6, high …
  5. … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300 - 400 °C. Old Hardfacing layers should …
  6. … for welding grey, malleable, nodular and phosphorus cast iron. Preheat is not necessary. Heat input is low which favors limited heat …
  7. … and corrosion resistance even in seawater. Welding instructions: - Preheating for sections >6 mm from 150 till 300 ºC is recommended. Use …
  8. … better galling resistance. Normally to obtain adequate ductility, preheat and post-weld heat-treatment are required . AA 410 is a …
  9. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good …
  10. … extreme high strength with excellent ductility and good weldabillity. Preheat and interpass temperature > 200°C …  1.7218, 1.7225 25 CD4, 13 …