1. … temperatures up to 600°C. The weld metal is resistant to high hydrogen pressure. … 12crmo19.5, GS-12crmo19.5, 1.7362, 1.7363     … E CrMo5 … A …
  2. … The weld puddle is amazingly fast freezing and therefore especially preferred in vertical down position with high speed and deep …
  3. Brand: Kobelco
    CEWELD Product: AA NiCro 625
    PREMIARC … 44 … DW-N625 …
  4. … of up to 550°C. Typical applications are in power plant construction, pressure pipe, turbine and boiler construction. The alloy is also used …
  5. … current, non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  6. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  7. … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. … 600 HB, T Fe 8 … MA 600 …
  8. … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected …
  9. … and well suited for low-temperatures, ductility down to -60°C. Preheating, interpass temperature and post weld treatment as required … 1.8914, 1.8927, 1.8931, 1.8928, 1.7147, 1.7149, 1.8734 S620Q, S620QL, S690Q, S690QL, S620QL1-S690QL1, 20MnCr65, 28CrMn4-3 L480 - L550, X65, X80, …
  10. …  high  strength, actual strength being dependent on heat treatment  Preheat,  interpass  temperature and PWHT will  be dependent  on …