1. … steam pipes and similar joints made of Cr-Mo alloyed steel. The weld metal is resistant to working temperatures up to 550°C. as for …
  2. … 4370 or OA MnCr is recommended in case of old layers or critical base metals.. … 64-68 HRc Hardfacing wire used in mining, agriculture and …
  3. … Latest generation basic slag guarantees optimum metallurgical quality and attractive welder appeal. The weld deposit …
  4. … The weld metal has excellent strength and oxidation resistance at high …
  5. … is a special alloyed copper wire for the MIG process. The weld metal is a Cu-Al-Ni bronze. Sound, pore free deposits on ferrous and … resistance to cavitations and stress corrosion cracking. … This filler metal with increased strenght and corrosion properties is verry wel …
  6. … 4370 or OA MnCr is recommended in case of old layers or critical base metals.. … 60-70 HRc Hardfacing wire used in mining, agriculture and …
  7. … High-alloyed tubular wire for metal spray on a C-Cr carbide basis for hard and corrosion resistant …
  8. … Usually combined with AlSi12 or AlSi5 filler metal. … Brazing for Aluminium and Aluminium Alloys with a working … range from 350 to 550 °C. Usually combined with AlSi12 or AlSi5 filler metal. … Alu-Flux … 18496: FL20 …
  9. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat resistant up …
  10. … production process the hydrogen content is below HD<3ml/100g weld metal even after long storage. … CuNi, Reh ≤ 460MPa ISo 15608: 1.4 …