1. … Submerged arc welding wire for fine grain steels where high impact values are required at low temperatures. … …
  2. … Higher corrosion resistance then standard Duplex steels with also higher mechanical properties due to the addition of Nitrogen. … Welding wrought, forged or cast super duplex stainless steels for service in the as-welded Condition. Heterogeneous welding between super duplex stainless steels and dissimilar welds between other stainless and mild or low …
  3. … for welding fine grained similar alloyed high yield strength steel > 960 MPa in case high impact values are required at sub …
  4. … chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, 20% Ni types. 310 has good general oxidation …
  5. … grain coarsening. Absence of stabilization means that this steel is distinctly vulnerable to sensitization phenomenon during …
  6. … Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production process the …
  7. … A stainless steel alloy for the assembly and cladding of 17% chromium alloys and … offers high hardness and wear resistance. … 1.4122 (G)X35CrMo17, Cast steels … 1.4115 … MA 4115 … A 5.9: ER430 … 14343-A: G 17 …
  8. … Ceweld SP NiAl is recommended. Suited for wear parts subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The …
  9. … Corrosion resistance is higher than 5%Cr-0.5%Mo steels requirements. To be used with shielding gas Ar+O2.   … For matching 9%Cr-1%Mo creep resisting martensitic steels ASTM: A182 Gr F9, A199 Gr T9 , A213 Gr T9 , A217 Gr C12 , A234 …
  10. … in case of rebuilding but heat input should be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or rebuilding parts that are subject to high impact and rolling …