1. … Submerged arc welding wire for fine grain steels where high impact values are required at low temperatures. … …
  2. … for welding fine grained similar alloyed high yield strength steel > 960 MPa in case high impact values are required at sub …
  3. … Root is a thick basic-rutile coated electrode for welding low alloyed steels with tensile strength up to 510 N/mm2. Recommended for root …
  4. … Designed for welding heat resistant steels to sustain working temperatures upto 650 ˚C … For matching 5%Cr-0.5%Mo creep resisting ferritic steels GX12CrMo5 (1.7362), X12CrMo5 (1.7363), Upto 1180 MPa ASTM: …
  5. … A stainless steel alloy for the assembly and cladding of 17% chromium alloys and … offers high hardness and wear resistance. … 1.4122 (G)X35CrMo17, Cast steels … 1.4115 … MA 4115 … A 5.9: ER430 … 14343-A: G 17 …
  6. … Ceweld SP NiAl is recommended. Suited for wear parts subject to heavy abrasion. The interpass temperature should be maximum 250ºC. The …
  7. … content (less than 0.05%), to be used for welding creep resistant steels. … For 2.5%Cr-1%Mo-alloyed, heat-resistant, ferritic steels of the same type. 1.7380, 1.7379 10CrMo 9-10, G-17CrMo 9-10, …
  8. … Corrosion resistance is higher than 5%Cr-0.5%Mo steels requirements. To be used with shielding gas Ar+O2.   … For matching 9%Cr-1%Mo creep resisting martensitic steels ASTM: A182 Gr F9, A199 Gr T9 , A213 Gr T9 , A217 Gr C12 , A234 …
  9. … in case of rebuilding but heat input should be kept low (as for Mn steel, interpass temperature should be kept < 250 °C). … Rebuilding and joining cold straining Mn steels or rebuilding parts that are subject to high impact and rolling …
  10. … offers excelent weldabillity when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to …