1. … from porosity due to the special shaving process and cleaning method during production. AlMg5 is one of the most popular types within the …
  2. … root of the weld on the first pass and blankets the solidified weld during subsequent passes until the root surface temperature stays below …
  3. … in case of old layers or critical base metals. Equivalent in SMAW: Dur 64 … For fire gratings, sintering plants, augers and blast furnace …
  4. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Grey Cast Iron, Malleable cast iron, EN 1561: EN-GJL-100 (GG10) till EN-GJL-350 (GG35), EN 1562: EN-GJMB-350 (GTS 35) till EN-GJMB-550 (GTS 55), EN- GJMW-350 (GTW 35) till EN- …
  5. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast … EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350, GG10, GG15; GG20, GG25; GG30; GG35; GG40 EN 1562: EN-GJMB-350, EN-GJMB-550 , EN- GJMW-350, EN- GJMW-550 , GTS 35, GTS 55, GTW 35, …
  6. … in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing peddles, …
  7. … for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to … ISO 15608: 8.1  Austenit ≤ 19 % Cr 9%Ni ,TÜV 1000: Gr. 21 - 22 (29 max.350°C), 1.4301, 1,4306, 1.4307, 1.4308, 1.4311, 1.4312, 1.6900, 1.6901, …
  8. … alloy containing Nickel for more strength and bridging capability during brazing with excellent rebuilding properties.  Flux/Paste: …
  9. … that this steel is distinctly vulnerable to sensitization phenomenon during welding, even though martensite hogs a great amount of carbon …
  10. … and leaves a fine rippled shiny surface. Max. service temperature 350ºC. Corrosion resistance similar to low carbon CrNiMo(Mn,N)-steels. …