1. … parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the benefits of being relatively …
  2. … or toughness. Grade 5 is used in aircraft components such as landing gear, wing spars, and compressor blades. Its corrosion resistance …
  3. … wetting properties due to slag support especially in positional welding. Excellent weldabillity and suitable for use with ceramic backing …
  4. … crack resistant alloy with high mechanical properties and excellent welding characteristics. High impact strength at sub zero temperatures …
  5. … metal has low levels of tramp elements (eg. Sn, As, Sb and P) providing a low Bruscato Factor(X < 10 ppm)for temper embrittlement …
  6. … bead appearance without slag residues. Best to be used with welding flux FL 915 … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …
  7. … SA 904L is used for welding materials of similar chemical composition which are used for …
  8. … basis for hard deposits on parts subject to abrasion. Excellent bonding strength. Is an 1.3505 Steel type specially modified for spraying. …
  9. … without slag. Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production …
  10. … base material or old layers. Weldable without protective gas.Corresponding electrode: Dur 62 S … 64-68 HRc hardfacing alloy, Cement, Mineral …