1. … offers a easily machinable weld deposit with high ductility and no undercut. … Welding ductile, grey and malleable cast irons. Ni 99 can …
  2. … concentrated intensive arc with deep penetration characteristics in order to ensure sound joint welds with good X-ray quality.. … Reh ≤ 420 …
  3. … and excellent weldability on both AC and DC+. The weld deposit can undergo a high polish due to the low carbon content.  … ISO 15608: 8.1 …
  4. … exceeds the level typically present in alloy C22; it is therefore considered suitable for welding this group of alloys. Alloy 59 consumables …
  5. … responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, …
  6. … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall …
  7. … therefore sensitive to hot cracking. The temperature limits for use under intermittent oxidation depend on cycle frequency. In general the …
  8. … all weld metal requires no buffer layer except on materials considered critical or in case of old hardfacing layers. In this Situation … by grinding.Weldable without gas (open arc). (Also weldable under M21 mixed gas) … 54 HRc hardfacing alloy for wear resistant …
  9. … dan 3 ml/100gr lasmetaal was de basis voor deze nieuwe ontwikkeling. Onder de noemer Megafil 890R is deze draad sinds kort leverbaar, een … metaal en een basisch gevulde draad zijn al langere tijd leverbaar onder de noemer Megafil 1100M  en Megafil 745B . .... meer informatie … …
  10. … all weld metal requires no buffer layer except on materials considered critical. In this situation CEWELD® ER 100 S-G is recommended. … the base metal and is achieved in the first layer. For material considered critical to cracking we advise to buffer with one layer CEWELD® … 55-62 HRc hardfacing alloy against heavy impact and shock, bucket, loaders, crusher jaws, crusher cones, pumps, sand, snow scratchers, stone …