1. … resistant steels and steel casting for working temperatures up to 600°C. The weld metal is resistant to high hydrogen pressure. … …
  2. … have a tendency to embrittle in the temperature range of approx. 600-800° C. The interpass temperature should not exceed 300° C. … G-X40CrNiSi 27 4, AISI 327, 442, 446, ASTM A 297 HC UNS S44200, 44600, J92605, J93005, J92605  … 1.4820 … AA 4820 … 17633-A: TZ 25 4 M …
  3. … for creep resistant service for working temperatures up to 600º C.  … 2,25% Cr, 1% Mo  1.7015, 1.7131, 1.7147, 1.7380, 1.7337, …
  4. … and by grinding. The hardness of the weld deposit will degreas 20% at 600°C and has a nominal hardness of 49-53 HRc at room temperature. The …
  5. … of the weld deposit will degrees 16% at 300°C and about 30% at 600°C. The weld deposit is high heat resistant up to 900°C. DUR 6 …
  6. … developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good resistance to general …
  7. … wires have strength of more than 1500 MPa and some wires only have 600 MPa. But why is this so important?   … Stainless steel wires, Matt …
  8. … abrasion resistance can be kept up to working temperatures of 600 ºC ; the hardness is still 40-45 HRc at these temperatures. For …
  9. … Het hoge percentage Mangaan gekombineerd met 0,5% Molybdeen staan garant voor zeer stabiele mechanische waarden zelfs na … S3 NiMo1 , een massieve O.P. draad met 0,95% Nikkel en 0,5% Molybdeen die garant staat voor een vloeigrens van minimaal 550 N/mm2 en …
  10. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel … Alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … 2.4665 … Alloy X … A 5.14: ERNiCrMo-2 … 18274: S Ni 6002(NiCr21Fe18Mo9) …