1. … 9015-B9 (P92) is designed to weld equivalent ‘type T/P92 CrMo steels modified with 1,6% Tungsten to match the base metal creep …
  2. … (pure Argon for the Tig process) suitable for high strength fine grain steels in combination with excellent impact toughness at sub zero …
  3. … type for economic production of high-strength fine-grain structural steels up to 1100 MPa Yield Strength. Stable mechanical property values …
  4. … Kb that delivers a welding deposit of less hardness. Overlays on steel with high tensile strength have to be buffered with CroNi 29/9 HL …
  5. … Austenitic filler metal for stabilized and non-stabilized CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down …
  6. … spatter loss, easy slag removal. Suitable for economic welding of Mo-steels up to 500°C (932°F). … Typ 0,5Mo  ≤ 460 MPa,  ISO 15608: 1.2, …
  7. … sub zero temperatures down to -60°C. CTOD tested and suitable up to steel types with 460 MPa yield strength (such as S460), approved …
  8. … of high-strength and low temperature fine grained structural steels. Excellent welding properties in combination with FL 155 high … 700, Dilimax, Naxtra 70, 10CrMo9-10, 16NiCrMo12-6, high strenght steels with yield >690N/mm2, S500Q-S690Q, S500QL-S690QL, P500Q-P690Q, …
  9. … to crack, especially if the weld seams are not heat-treated.These steels are usually used for operating temperatures of up to 550°C. … … For similar 1.25%Cr-0.5%Mo-alloyed, heat-resistant, ferritic steels. 1.7335, 1.7242, 1.7337, 1.7357 13CrMo 4-5, 13CrMo 4-4, 16 …
  10. … Corrosion resistance is higher than 5%Cr-0.5%Mo steels requirements. To be used with shielding gas Ar+O2.   … For matching 9%Cr-1%Mo creep resisting martensitic steels ASTM: A182 Gr F9, A199 Gr T9 , A213 Gr T9 , A217 Gr C12 , A234 …