1. … CEWELD® 308L Tig has good general corrosion resistance. The alloy has a low carbon … UNS S30409, S32109, S34709, S30400, S32100, S34700   … 1.4316 … 308L Tig … A 5.9: ER308L … 14343-A: W 19 9 L …
  2. … and an excellent colour-uniformity after anodizing. CEWELD® AlMg3 Tig offers also good resistance against seawater. … Aluminium alloys: … EN AW 5754, EN AW 6060, EN AC 51100, EN AW 5454, EN AW 5251 … AlMg 3 Tig … A 5.10: ER5754 … 18273: S Al 5754 (AlMg3) …
  3. … corrosion, also in fuel-ash atmosphere containing sulfur and vanadium … ASTM B163, B166, B167, B168 with UNS N06690, IN657, Incoloy 671/800H … NiCro 72 Tig … A 5.14: ERNiCr-4 … 18274: S Ni 6072 (NiCr44Ti) …
  4. … properties and low fume, extreme subzero impact properties due to the TIG process. … Reh ≤ 420 MPa (67 ksi) ISO 15608: 1.2, 1.3, 2.1 1.5637, … X52, X56, X60, X65  Domex 315-460MC,MC Plus, ML    … 1.5125 … SG 2 Tig … A 5.18: ER 70S-6 … 636-A: W 46 5 W3Si1 …
  5. TIG/GTAW rod for T24 creep resistant steel. The T24 alloy is a modified … 213 Grade T24 A/SA 335 Grade P23 - A/SA 213 Grade T23 … ~1.7378 … P24 Tig … A 5.28: R90S-B24 … 21952-A: W ZCrMo2VNb …
  6. … cycling conditions exceeding 1200°C and carburized medias. Excellent fatigue strength and creep properties. The high chromium and aluminum … methanol and ammonia synthesis, Inconel alloy 693 … Nicro FM 53MD Tig … A 5.14: ERNiCrFeAl-1 … 18274: S Ni 6693(NiCr29Fe4Al3) …
  7. … CEWELD 310LMo Tig has been developed primarly to cope with the severe corrosion … 25 22 2, 2RE69, 3R60U.G (Sandvik),Cronifer 25.25.LCN … 1.4466 … 310LMo Tig … A 5.9: ~ER 310 … 14343-A: W 25 22 2 N L …
  8. … Special alloyed copper rods for Tig welding. The weld metal is a Cu-Al bronze. Sound, pore free … CuZn20Al2, Werkstoff Nr : 2.0916 - 2.0920 - 2.0960 … 2.0937 … CuAl9Fe Tig … A 5.7: ERCuAl-A2 … 24373: Cu 6180 / CuAl10Fe …
  9. … CEWELD® 316LSi Tig offers good general corrosion resistance, particularly to corrosion … 444 S31640, S31603, S31653, S31600, S31630, S44400 … 1.4430 … 316LSi Tig … A 5.9: ER316LSi … 14343-A: W 19 12 3 LSi …
  10. … Saving the cost for back shielding gas and purging time makes AA 316L Tig a very economical option. … ISO 15608: 8.1  Austenit ≤ 19 % Cr , … UNS S31603, UNS S31653, UNS S31600, UNS S31635   … 1.4430 … AA 316L Tig … A 5.22: E316LT1-1 …