1. … In this  Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to extreme heavy abrasion …
  2. … (internal shielding gas). As they produce a slag, they are not recommended for multi-pass welding. … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) …
  3. … The alloy has a low carbon content, making it particularly recommended where there is a risk of intergranular corrosion. … ISO 15608: …
  4. … in the first layer. A buffer layer with OA 4370 or OA MnCr is recommended in case of sensible basematerial or old Hardface-layers. … 59-62 …
  5. … Ti can be used for a working temperature of up to 450ºC. The recommended preheat temperature is 200ºC - 300°C unless the base material …
  6. … preheat temperature, interpass temperature and PWHT) will be dependent on the base material being welded, including its thickness, and …
  7. … already a High hardness in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without …
  8. … Grâce au processus de fabrication et au double recuit à 580ºC pendant le processus d'étirage, la teneur en hydrogène de nos fils …
  9. … become part of the weld deposit, Metal core fluxcored wires are recommended in spray arc to obtain the best results. The torch angle should …
  10. … not be deposited. A Buffer layer with OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. … 60-70 HRc …