1. …  high  strength, actual strength being dependent on heat treatment  Preheat,  interpass  temperature and PWHT will  be dependent  on …
  2. … current, non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  3. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  4. … to enhance properties. Low carbon (C) helps minimize grain boundary precipitation to maintain corrosion-resistance in the heat-affected …
  5. … and well suited for low-temperatures, ductility down to -60°C. Preheating, interpass temperature and post weld treatment as required …
  6. … risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300-400°C. … 600 HB, T Fe 8 … MA 600 …
  7. … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by …
  8. … current, copper coated core wire and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you …
  9. … and well suited for low-temperatures, ductility down to -50°C. Preheating, interpass temperature and post weld treatment as required …
  10. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. Outstanding slag release. … Rebuilding worn …