1. … developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good resistance to general …
  2. … of the weld deposit will degrees 16% at 300 °C and about 30% at 600 °C. The weld deposit is high heat resistant up to 900 °C.  … …
  3. … excellent ductility.  Long term use at working temperatures between 600°C and 800°C should be avoided. … Ni 6625 / NiCr22Mo9Nb / 2.4831 … - NiCr21Mo - 8XNi9 ASTM: A 533 Gr1 UNS: S31254 - N08800 - N08810 - N06600 - N06625 - N08825 - N08926 - N08020 Alloy 254 SMO - Alloy 800 - Alloy 800H - Alloy 600 - Alloy 625 - Alloy 825 - Sanicro 28 … NiCro 625 Tig … A 5.14: …
  4. … subsequent passes until the root surface temperature stays below 600 degrees F. Backup shielding also should be used on the back surface …
  5. … and by grinding. The hardness of the weld deposit will degrees 20% at 600°C and has a nominal hardness of 49-53 HRc at room temperature. The …
  6. … oxidation, at service temperatures ranging from 1200°F (650°C) up to 1600°F (870°C) … AMS 5708, 5709, 5706, 5707, 5704, 5544, 5586. PWA 1005, …
  7. … resistant steels and steel casting for working temperatures up to 600°C. The weld metal is resistant to high hydrogen pressure. … …
  8. … innovativer Schweißprozesse und -verfahren zu schaffen. Der Standort (600 m2) bietet Platz für die hochwertigsten und innovativsten …
  9. … have a tendency to embrittle in the temperature range of approx. 600-800° C. The interpass temperature should not exceed 300° C. … G-X40CrNiSi 27 4, AISI 327, 442, 446, ASTM A 297 HC UNS S44200, 44600, J92605, J93005, J92605  … AA 4820 … 17633-A: TZ 25 4 M M21 1 …
  10. … and by grinding. The hardness of the weld deposit will degreas 20% at 600°C and has a nominal hardness of 47-52 HRc at room temperature. The …