1. … positions for diameters 2.4 and 3.2mm. Diameters < 4.0mm excellent in down position. … Joining Duplex, Superduplex, super austenitic …
  2. … are controlled to lower levels in this alloy. Suitable only in down-hand positions. … 1.4465, 1.4500, 1.4505, 1.4506, 1.4519, 1.4531, …
  3. … welding characteristics. High impact strength at sub zero temperatures down to -60 °C. Weldable with Co2 and Mixed gas. … Reh < 690 MPa Iso …
  4. … at high currents. The weld deposit shows reliable impact properties down to -60°C. Particularly suitable for MAG orbital welding and for …
  5. … CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to nitric acid. … ISO 15608: 8.1 …
  6. … weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …
  7. … purity, superior hot cracking and corrosion resistance. CVN toughness down to –120 °C, resistant to intergranular corrosion up to 400 °C. …
  8. … manual and (semi- and fully) mechanized welding. Good quality values down to -40°C. Low spatter losses with excellent slag removability. …
  9. … High strength weld deposit with good impact properties down to -60°C. S3 NiMo1 can be used in combination with FL 851 and FL …
  10. … a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you can not control the cooling speed …