1. … layer with OA 4370 or OA MnCr is recommended in case of sensible base material or old hardface-layers. Weldable without protective gas. …
  2. … wires with better arc stability and improved wetting properties with less spatters. … Ni 6625 / NiCr22Mo9Nb / 2.4831 1.4547 - 1.4876 - …
  3. … OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing peddles, coke wear plates, Fan blades, screw conveyors, pumps etc. … OA 57 …
  4. … wire is used for welding matching, and similar, composition base materials. … 30CrMoV12, 55NiCrMoV7, 55CrNiMo4 … SG CrMnMo Tig … A …
  5. … and when used to join Monel K-500 it has lower strength then the base metal.  … 2.4360, 2.4375, NiCu30Fe, NiCu30Al, Monel 400, R405, …
  6. … CEWELD SA 309LMo strip is stainless steel strip for cladding overlay applications. Latest generation …
  7. … of titanium with carbon maintains a low level of free carbon and enables the filler metal to be used with Nickel 201. The weld metal has … of filler metal NiTi 3 include joining Nickel 200 and 201 to stainless steels, copper-nickel alloys, and Monel alloys. It is also used …
  8. … Very good welding characteristics and not sensitive for old and rusty base-materials, good mechanical properties and stable arc for welding …
  9. … CEWELD 410 is a martensitic stainless steel that is heat-treatable. It has a nominal weld metal …
  10. … CEWELD® OA 4370 or CEWELD® OA MnCr is recommended in case of sensible basematerial or old hardface-layers. Weldable without protective gas. … …