  • PRODUCT SPECIFICATIONS
  • PACKAGING
Type
Carbide powder, agglomerated and sintered
classification
EN ISO
14232-1 WC-Ni 88/12
Anwendungen
carbide powder for wear resistant coatings produced by flame-, plasma or hig hvelocity- flame-spraying (HVOF). Tungsten-Carbide-Nickel-coatings are resistant to abrasion and oxidation. In comparison with WC-Co layers they show an improved corrosion resistance in aqueous solutions. Plasma sprayed coatings can achieve a hardness of up to 1000 HV0.1 and tensile strength acc. to DIN 50160 of 60 N/mm². The maximum operating temperature is 750°C.
Type
Carbide powder, agglomerated and sintered
Anwendungen
carbide powder for wear resistant coatings produced by flame-, plasma or hig hvelocity- flame-spraying (HVOF). Tungsten-Carbide-Nickel-coatings are resistant to abrasion and oxidation. In comparison with WC-Co layers they show an improved corrosion resistance in aqueous solutions. Plasma sprayed coatings can achieve a hardness of up to 1000 HV0.1 and tensile strength acc. to DIN 50160 of 60 N/mm². The maximum operating temperature is 750°C.
Eigenschaften

Crystal size of WCApparent Density (ISO 3923-2 )Particle Size Range in μm Particle Shape 2.5 μm

FSSS4.3 – 5.4 g/cm22/5 - 38/15 - 53/22 Preponderant spherical 

Klassifikation
EN ISO
14232-1 WC-Ni 88/12
Geeignet für

Augers, impellors, shafts, hydraulics, pulling equipment, fan blades etc.

Schweißpositionen
PC
Rücktrocknung
Not required
Gas acc. EN ISO 14175
None
Analyse
Ni WC
12 88
Packing info
Powder 8812-Ni 
Packaging KG/unit EanCode