1. … hardness and is resistant against metal-metal wear and high surface pressure.  … 13% Cr- 4%Ni-0,5% Mo Steel  1.4317, 1.4313, …
  2. … free from porosity even on old and or otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you …
  3. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  4. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low …
  5. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Rebuilding worn machine parts, Rails, …
  6. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with OA 4370 or …
  7. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good …
  8. … N/mm2 est déjà extrêmement difficile et les restrictions T-8/5 sont presque impossibles à respecter dans la pratique. Habituellement, des …
  9. … exceeding 500 MPa in sweet and salt water makes AquaForce MG the preferred choice by professional divers. … Reh ≤420 MPa (60 ksi) ISO …
  10. Brand: Kobelco
    CEWELD Product: AA NiCro 625
    PREMIARC … 44 … DW-N625P …