1. … levels of tramp elements (eg. Sn, As, Sb and P) providing a low Bruscato Factor(X< 10 ppm)for temper embrittlement resistant applications. … For matching 1.25%Cr0.5%Mo creep resisting ferritic steels.  …
  2. … materials of similar chemical composition which are used for fabrication of equipment and vessels for handling of sulfuric acid and many chloride containing media. This fluxcored wire may also find applications for joining Type 317L material where improved corrosion …
  3. … materials of similar chemical composition which are used for fabrication of equipment and vessels for handling of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where improved corrosion …
  4. … levels of tramp elements (eg. Sn, As, Sb and P) providing a low Bruscato Factor.(X<10 ppm)for temper embrittlement resistant applications. … For matching 2.5%Cr1%Mo creep resisting ferritic steels EN: …
  5. … materials of similar chemical composition which are used for fabrication of equipment and vessels for handling of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where improved corrosion …
  6. … de sécurité et de qualité les plus strictes, telles que les certifications SCC-P et ISO 9001-2008. Outre notre siège social à Stellendam, nous disposons de plusieurs sites, notamment à Anvers, en Roumanie, au Portugal, aux Caraïbes et au …
  7. … materials of similar chemical composition which are used for fabrication of equipment and vessels for handling of sulfuric acid and many chloride containing media. This filler metal may also find applications for joining Type 317L material where improved corrosion …
  8. … usually used for operating temperatures of up to 550°C. Typical applications are in power plant construction, pressure pipe, turbine and … of accompanying elements (Sn, As, Sb, P) in the wire ensures a low Bruscato factor (X < 10 ppm) and therefore insensitivity to temper …
  9. … CEWELD® Alloy 263 should be used used for applications up to about 1650°F (900°C). Its oxidation resistance is … to combine good age-hardened strength properties with excellent fabrication characteristics in the annealed condition. CEWELD® Alloy …