1. … Good resistance against hot cracking due to the high Mo content. During build-up welding, the weld metal already achieves approximately …
  2. … old layers. Weldable without protective gas.Corresponding electrode: Dur 62 S … 64-68 HRc hardfacing alloy, Cement, Mineral mixing, hammers, …
  3. … from porosity due to the special shaving process and cleaning method during production. AlMg5 is one of the most popular types within the …
  4. … root of the weld on the first pass and blankets the solidified weld during subsequent passes until the root surface temperature stays below …
  5. … in case of old layers or critical base metals. Equivalent in SMAW: Dur 64 … For fire gratings, sintering plants, augers and blast furnace …
  6. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Grey Cast Iron, Malleable cast iron, EN 1561: EN-GJL-100 (GG10) till EN-GJL-350 (GG35), EN 1562: EN-GJMB-350 (GTS 35) till EN-GJMB-550 (GTS 55), EN- GJMW-350 (GTW 35) till EN- …
  7. … de sortir aussi droit que possible de la torche. Tous les fils de soudure Ceweld® sont suivis d'un stricte contrôle "Cast" et pour certains …
  8. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast … EN-GJL-100, EN-GJL-150, EN-GJL-200, EN-GJL-250, EN-GJL-300, EN-GJL-350, GG10, GG15; GG20, GG25; GG30; GG35; GG40 EN 1562: EN-GJMB-350, EN-GJMB-550 , EN- GJMW-350, EN- GJMW-550 , GTS 35, GTS 55, GTW 35, …
  9. … in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing peddles, …
  10. … souhaitez utiliser pour vos applications de rechargement. Avec une dureté de plus de 2400 HV et une surface extrêmement rugueuse, des … la buse de gaz (trailing) où les particules font partie du bain de soudure en cours de solidification. Lors de la journée thématique …