1. … Solid welding wire that combines high hardness with very good corrosion …
  2. … range of alloys. Thicker sections should be preheated (150°C) prior to welding. … Aluminium alloys: AlMg3, AlMg4, AlMg5,AlMgSi0.5, AlMgSi1; …
  3. … Solid drawn ,corrosion-resistant, chromium-nickel wire for welding heat-resistant austenitic steels of the 25% Cr, 20% Ni …
  4. … Mo content, with low carbon content (less than 0.05%), to be used for welding creep resistant steels. … For 2.5%Cr-1%Mo-alloyed, …
  5. … between 30 and 50 (FN). Excellent for use in position and down hand welding. Excellent against pitting and stress corrosion.PREN above 35 …
  6. … as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool 55ºC/ hour to 620ºC, than Air Cool for 8 hours.   … …
  7. … Excellent welding properties with high buildup capacity and low dilution rate … … Cladding against high temperature, radiant heater tubes, furnace rolls, muffles in bright annealing furnaces (H2 atmosphere), rotary kilns, waste gas components, hydrogen …
  8. … High chromium-alloyed welding wire (ER 327-ER 329) based on a 25% Chromium and 4% Nickel …
  9. … to buffer with an electrode like CEWELD E DUR 350 Kb that delivers a welding deposit of less hardness. Overlays on steel with high tensile …
  10. … Special alloy for welding aluminium-magnesium based alloys with maximum 5% Mg. Zirconium …